胡志刚、赵彦华、孙玉虎 等 4 位作者2007-02-01Teshugang
LF (ladle furnace)refining is a key metallurgical process for steelmaking cold rolled low carbon steel in BOF-LF-CSP flow sheet. The electric characteristics of a 120 t LF with 20 MW transformer and the power supply curves have been studied and optimized by established optimizing model to decrease refining time and im…
刘坤、朱苗勇、高茵 等 4 位作者2007-02-01Teshugang
The numerical simulation of jet flow field of inner and out of Laval tube has been carried out by commercial software CFX4. 4, and the fluid flow distribution of axis symmetry turbulence jet out of tube with different stagnation pressure was analyzed to verify the k-ε turbulence model. Results showed that at environme…
徐芳泓、龚伟、姜周华2007-02-01Teshugang
A charge partition model for stainless steel smelting by K-OBM-S process at Taiyuan Steel has been established by a linear programming method including 13 decision variables in the model, minimum cost charge partition selected to be objective function and a set of linear equality and inequality about variable as restr…
刘守显、罗海文、雍岐龙 等 5 位作者2007-02-01Teshugang
The controlled rolling and cooling test for a V-Nb-Ti microalloying X100 pipeline steel(0.057C,1.84Mn, 0.25Mo) has been caried out by φ350 mm 4 roll mill in laboratory.Results showed that with initial rolling temperature 1100 ℃,finishing temperature 800~900 ℃ and end cooling temperature 100~400 ℃ the structure of X100…
徐芳泓、孙铭山、丁伟中 等 4 位作者2007-02-01Teshugang
The nitrogen removal from 0. 02% C molten steel in argon direct current (DC) glow plasma has been tested by a 25 kg vacuum induction furnace and the effect of argon glow plasma on kinetics of nitrogen removal from molten steel was studied. Results showed that the nitrogen removal speed and efficiency from molten steel…
廖舒纶、张立文、岳重祥 等 5 位作者2007-02-01Teshugang
The two- and three-dimensional models of 12 pass continuous rolling process for 150 mm × 150 mm billet to φ32 mm rod have been established by commercial finite element software MSC .Marc,and the simulation results of cross section shape,temperature of rolling stock during rolling process by two- and three-dimensional…
毛伟强、宋志刚、王华昆 等 7 位作者2007-02-01Teshugang
The plane-strain compression test with strain rate 10 s-1 and 50 s-1 at 900~1200 ℃ for forged dual phase stainless steel 00Cr22Ni5Mo3N has been carried out by Gleeble 3800 simulation test machine.Test results showed that with increasing deformation temperature the peak resistance to deformation of the dual phase steel…
冯巍、胡明谦、李德强 等 5 位作者2007-02-01Teshugang
The bubbles movement behavior in mold with cast speed 1.1 m/min,nozzle submerged depth 160 mm and gas flow rate in nozzle 0~15 L/min,and the effect of bubbles movement on impact depth,liquid level fluctuation and surface naked of mold powder have been studied by physical model in the ratio 0.4 to 1300 mm × 230 mm slab…
陶建军、朱惠刚、吴小林2007-02-01Teshugang
The effect of magnetic stirring current on carbon segregation of 180 mm×180 mm cast billet of gear steel 20CrMnTiHl and the effect of change of residual B content in steel during refining and casting on hardenability of steel have been tested and analyzed. Results showed that as magnetic stiring current decreased from…
姜静、李华德、孙铁 等 4 位作者2007-02-01Teshugang
BP ( Back Propagation) algorithm and genetic algorithm are combined into hybrid genetic algorithm of which the algorithm steps are first to locate a favorable searching region by genetic algorithm, then to search optimal coefficients in the located region by BP algorithm. An 100 t arc furnace end aim temperature neura…
武建平、贾建平、王自东2007-02-01Teshugang
The modified containing tungsten added V-N microalloying Cr5W tool steel-0.70~0.90C,≤1.00Si,0.20~0.60Mn,4.50~5.50Cr,1.00~1.50W,≤0.15Mo,≤0.3V,300×10-6~350×10-6N has been developed. Test results indicated that the structure of modified Cr5W steel quenched at 960 ℃ was martensite + carbide,of which the average HRC hardne…
魏果能、俞峰、许达2007-02-01Teshugang
The structure and properties of GCr4 bearing steel- 1.00%C,0.40%Cr,0.03%Mo,0.034%Al,10 × 10-6[O] heat treated by cross section induction heating and quenching (840±10)℃ + tempering (150~160 ℃) have been tested and researched. Results showed that after heat treated the case structure of CCr4 steel consisted of twinned…
包丽明、刘坤、吕国成 等 4 位作者2007-02-01Teshugang
According to production condition of an 180 t oxygen converter, the hydraulic simulation test of 1/15 model of oxygen top blown converter has been carried to get the effect of blown process parameters on bath. Results showed that as top blown gas flow rate was m 15.5 m3/h the change of oxygen lance position and gas fl…
颜飞、徐洲、金冰忠2007-02-01Teshugang
The wear properties and wear surface morphology of three kinds of plastic die steel STAVAX (0.37C, 13.40Cr,0.31V), M330 (0.36C,12.88Cr,0.15Mo) and N702 (0.05C,16.30Cr,4.00Cu,4.00Ni,0.34Nb)with excellent corrosion resistance have been studied by M200 ring-block wear testing machine and scanning clectron micro-scope.Res…
池武2007-02-01Teshugang
The process of 100t DCEAF+LF+VD-220 mm×220 mm continuous billet -rolling mill to rollφ 55~70 mm GCr15 bearing steel bar has been developed. Process test results showed that with overheating temperature of molten steel during continuous casting ≤35 ℃,heating time of 220 mm×220 mm billet ≥8 h,rolling reduction 12.58~ 20…
赵舸、何平2007-02-01Teshugang
An excellent arithmetic for flow rate control - expert and alterable parameter PID control arithmetic has been developed by combining theory with practice to realize optimal control for bottom blowing flow rate. The practical application of 30 ~ 120 t top and bottom combined blown converter indicated that the expert a…
常立忠、李正邦2007-02-01Teshugang
According to characteristics of electroslag remelting (ESR) of steel, the unsteady-state model for ESR slab ingot has been established to simulate the temperature field of slab ingot during ESR with different remelting speed and analyze the effect factors on metal pool depth. Simulation results showed that during reme…
杜珊、闫绍维、王硕明 等 4 位作者2007-02-01Teshugang
The behavior,characteristics,amount and transformation of microinclusion in bearing steel at each procedure of 45t BOF-LF-VD-CC flow sheet at Shijiazhuang Steel have been studied by added tracer elements.Results showed that inclusions in steel before LF refining were gradually transformed from blocky Al2O3chromic-sili…
计云萍、金自力、王权 等 5 位作者2007-02-01Teshugang
Key words:CSP Cold Rolling Sheet,Bell Type Fumace,Annealing,Sticking
雷秀华、邓通武2007-02-01Teshugang
The non-quenched and tempered steel 36Mn2V (0.34~0.38C,1.45~1.70Mn, 0.11~0. 16V, 0.020Als)was produced by hot metal pretreated -120 t converter melting -predeoxidizing by Pl deoxidizing agent with main component CaC2then alloying-LF + RH refining-280 mm × 380 mm billet concasting process at Panzhihua Steel. The analys…