J. I. Fernández-Golfín Seco、M. Rafael Díez Barra1997-06-01Materiales de Construccion
Four different strategies of surface coating (based on 80 g m2 melamin impregnated papers) were used on 19 mm thick commercial MDF panels to assess its reological behaviour under cyclic humidity conditions (20ºC 30 % rh-20ºC 90 % rh). Three different levels of stress (20 %, 30 % and 40 %), based on the ultimate load i…
J. L. Álvarez Cabrera、F. Urrutia、D. Lecusay 等 4 位作者1997-06-01Materiales de Construccion
The possibility of recycling construction rubble, its technical and economic effectiveness, and the social and ecological impact they provide for our society is the reason and the starting point for an optimal exploitation of this aggregate in the manufacture of masonry mortar, since it has the same inherent propertie…
Zako, M.、Takano, N.、Takeda, N. 等 4 位作者1997-06-01Science and Engineering of Composite Materials
作者信息未提供1997-06-01Applied Rheology
作者信息未提供1997-06-01Applied Rheology
作者信息未提供1997-06-01Applied Rheology
Schieber J.、Fischer P.、Kroger M.1997-06-01Applied Rheology
Aksel M.1997-06-01Applied Rheology
Kuhn E.1997-06-01Applied Rheology
Hyakutake, Hiizu、Yamamoto, Toshihiro1997-06-01Science and Engineering of Composite Materials
Ochiai, Shojiro、Sawada, Takehiro、Hojo, Masaki1997-06-01Science and Engineering of Composite Materials
Kimura, T.、Nakanishi, K.1997-06-01Science and Engineering of Composite Materials
M. T. Blanco-Varela1997-06-01Materiales de Construccion
In the present work, the depicted coat that covers some of the mortars exposed to weathering in the Medina Azahara archaeological site is .studied. That coat is characterized from the compositional and physical viewpoint and the main causes for its decay are determined. The depicted coat is formed by cal cite and iron…
Nowak J.、Gutbrod M.1997-06-01Applied Rheology
A. Fernández-Jiménez、F. Puertas1997-06-01Materiales de Construccion
The influence of activator solution concentration on hydration kinetics of an alkaline activated blast furnace slag has been studied. The alkaline activator used was a mix of waterglass (Na2SiO3∙nH2O) and NaOH solution (of variable concentration). Final activator concentrations were 3,4 and 5 % Na2O wt. with respect t…
作者信息未提供1997-06-01Applied Rheology
Equipo Editorial1997-06-01Materiales de Construccion
作者信息未提供1997-06-01Applied Rheology
作者信息未提供1997-06-01Science and Engineering of Composite Materials
Saito, Atsushi、Takahashi, Hiromasa1997-06-01Science and Engineering of Composite Materials